1 - Erosion-corrosion of electrodeposited superhydrophobic Ni-Al2O3 nanocomposite coatings under jet saline-sand slurry impingement (چکیده)2 - Proposed stability product criterion for open hemispherical metastable pits formed in the crevices of different aspect ratios (l/d) on 316L stainless steel in 3.5% NaCl solution (چکیده)
3 - Hot corrosion of Inconel 625 wrought alloy and weld overlay on carbon steel by gas metal arc welding in 47 PbSO4-23 ZnO-13 Pb3O4-7 PbCl2-5 CdO-5 Fe2O3 molten salt mixture (چکیده)
4 - High temperature oxidation behaviour of AISI 321 stainless steel with an ultrafine-grained surface at 800 °C in Ar–20 vol.% O2 (چکیده)
5 - Access to nanocrystalline, uniform, and fine-grained Ni-P coating with improved anticorrosive action through the growth of ZnO nanostructures before the plating process (چکیده)
6 - Eddy current technique as a nondestructive method for evaluating the degree of sensitization of 304 stainless steel (چکیده)
7 - The influence of the crevice induced IR drop on polarization measurement of localized corrosion behavior of 316L stainless steel (چکیده)
8 - Microscale investigation of the correlation between microstructure and galvanic corrosion of low alloy steel A508 and its welded 309/308L stainless steel overlayer (چکیده)
9 - Investigation of zinc as a scale and corrosion inhibitor of carbon steel in artificial seawater (چکیده)
10 - New insights into the effects of surface nanocrystallization on the oxidation of 321 austenitic stainless steel in a humid oxygen environment at 1000 °C (چکیده)
11 - Correlation of surface Volta potential with galvanic corrosion initiation sites in solid-state welded Ti-Cu bimetal using AFM-SKPFM (چکیده)
12 - Enhanced corrosion protection of mild steel by the synergetic effect of zinc aluminum polyphosphate and 2-mercaptobenzimidazole inhibitors incorporated in epoxy-polyamide coatings (چکیده)
13 - Pitting corrosion of martensitic stainless steel in halide bearing solutions (چکیده)
14 - Corrosion protection of the reinforcing steels in chloride-laden concrete environment through epoxy/polyaniline–camphorsulfonate nanocomposite coating (چکیده)
15 - Microstructure and corrosion characterization of the interfacial region in dissimilar friction stir welded AA5083 to AA7023 (چکیده)
16 - Investigation of the effect of solution annealing temperature on critical pitting temperature of 2205 duplex stainless steel by measuring pit solution chemistry (چکیده)
17 - A statistical study on the effect of annealing temperature on pitting corrosion resistance of 2205 duplex stainless steel (چکیده)
18 - The effect of dichromate ion on the pitting corrosion of AISI 316 stainless steel Part II: Pit initiation and transition to stability (چکیده)
19 - Effect of grain size on pitting corrosion of 304L austenitic stainless steel (چکیده)
20 - Water-base acrylic terpolymer as a corrosion inhibitor for SAE1018 in simulated sour petroleum solution in stagnant and hydrodynamic conditions (چکیده)
21 - The role of constituent phases on corrosion initiation of NiAl bronze in acidic media studied by SEM–EDS, AFM and SKPFM (چکیده)
22 - A comparative H2S corrosion study of 304L and 316L stainless steels in acidic media (چکیده)
23 - The effect of dichromate ion on the pitting corrosion of AISI 316 stainless steel. Part I: Critical pitting temperature (چکیده)
24 - Correlation between sensitisation and pitting corrosion of AISI 403 martensitic stainless steel (چکیده)
25 - Investigation on the effect of nitrate ion on the critical pitting temperature of 2205 duplex stainless steel along a mechanistic approach using pencil electrode (چکیده)
26 - Pitting corrosion of cold rolled solution treated 17-4 PH stainless steel (چکیده)
27 - EIS assessment of critical pitting temperature of 2205 duplex stainless steel in acidified ferric chloride solution (چکیده)
28 - Establishing a correlation between interfacial microstructures and corrosion initiation sites in Al/Cu joints by SEM–EDS and AFM–SKPFM (چکیده)
29 - Electrochemical and quantum chemical assessment of two organic compounds from pyridine derivatives as corrosion inhibitors for mild steel in HCl solution under stagnant condition and hydrodynamic flow (چکیده)
30 - In situ inhibitor synthesis from admixture of benzaldehyde and benzene-1,2-diamine along with FeCl3 catalyst as a new corrosion inhibitor for mild steel in 0.5 M sulphuric acid (چکیده)
31 - A comparative study of critical pitting temperature (CPT) of stainless steels by electrochemical impedance spectroscopy (EIS), potentiodynamic and potentiostatic techniques (چکیده)
32 - Theoretical and electrochemical assessment of inhibitive behavior of some thiophenol derivatives on mild steel in HCl (چکیده)
33 - Critical pitting temperature dependence of 2205 duplex stainless steel on dichromate ion concentration in chloride medium (چکیده)
34 - Correlation between critical pitting temperature and degree of sensitisationon alloy 2205 duplex stainless steel (چکیده)
35 - AGGRESSIVE EFFECTS OF PITTING “INHIBITORS” ON HIGHLY ALLOYED STAINLESS STEELS (چکیده)
36 - The mechanism of lacy cover formation in pitting (چکیده)
37 - Critical pitting temperature (CPT) assessment of 2205 duplex stainless stell in 0.1 M NaCl at various molybdate concentrationsl (چکیده)
38 - Improving the corrosion behaviour of powder metallurgical 316L alloy by prepassivation in 20% nitric acid (چکیده)
39 - Tuning DOS measuring parameters based on double-loop EPR in H2SO4 containing KSCN by Taguchi method (چکیده)
40 - Dependence of the Critical Pitting Temperature on surface roughness (چکیده)
41 - Deterioration in critical pitting temperature of 904L stainless steel by addition of sulfate ions (چکیده)